  • High transparency mold making silicone rubber

    High transparency mold making silicone rubber

    10: 1 two-component liquid silicone rubber is an addition type non-toxic and tasteless transparent liquid silicone mold rubber, the product has a high transparency after curing, high tear resistance, almost no shrinkage, Good stability, good mold release, no deformation and so on. It is an elastic mold material for filled with AB water, PU, epoxy resin, 815 resin, Polly resin, PT, ABS material and so on.

     


    Product technical data

    Item number

    Color

    Hardness(A)

    Viscosity(cps)

    Tear strength(KN/m)

    Tensile strength

    (Mpa)

    Elongation (%)

    Mixing time(Min)

    IOTA-

    1310

    High transparent

    10±2

    25000±5000

    4

    2.88

    500

    60±10

    IOTA-

    1320

    High transparent

    20±2

    45000±5000

    6

    3.10

    450

    60±10

    IOTA-

    1330

    High transparent

    30±2

    65000±5000

    9

    4.15

    350

    60±10

    IOTA-

    1340

    High transparent

    40±2

    80000±5000

    13

    3.61

    300

    60±10



    Products Procedure

    1. Mixing: The A and B rubber 1: 1 weight ratio mix and stir evenly.

    2. Discharge bulbs: For high requirements should be evacuated discharge bubbles, otherwise the mold will have bubbles.

    3. Material pouring: pour the mixing the stirred liquid silicone into the mold box.


    Precautions For Use

    1. Before large-scale use, please do small amount of trial, familiar with the production skills to avoid errors.

    2. Do according to the manufacturer's instructions ratio for quantity, and the weighing accuracy, please remember that the ratio is by weight rather than volume. After the mixing of AB silicone rubber, stir it fully to avoid not cure or incomplete cure.

    3. When make the mold frame, if 502 glue is applied, pour the mixing silicone rubber after half an hour or put it into oven at 50℃ for 10 minutes, to prevent 502 glue and silicone poisoning to make it not cure.

    4. To accelerate the curing time, heating method can be used to speed up the curing rate of silicone rubber.

    5. When mixing the AB silicone, mixing in the same direction. When pour glue, take a little bit of the higher and same position on the female die on the same position, let the glue flow flat on the master die, it will increase the flow time of the glue to reduce the bubble.  Generally, the silicone in hardness higher than 20, it will need to do vacuum pumping before use.

    6. 1:1 Additional products will have toxic reaction with tin, phosphorus, ammonium, chlorine, carboxylic acids, thiol, hydroxyl and other compounds. It is forbidden to contact with such compounds to avoid the occurrence of non-curing.



Feedback to "Iota Silicone Oil (Anhui) Co., Ltd."

  • *Name:
    *Contacts:
    *Content:
    *Code:    验证码

    Iota Silicone Oil welcome your message...

New Products

皖ICP备14007495号

Copyright © 2000-2024 Iota Silicone Oil (Anhui) Co., Ltd, All Rights Reserved